In this note...
A three turn helical coil is used to heat the aluminum pulley. The pulley is heated to 464 ��F (240 ��C) in 20 seconds to expand the inner diameter and then the inner bearing is inserted to form the completed part.
Get your Free shrink-fitting Application Note
'shrink-fitting aluminum pulley to insert inner bearing'
See how we've applied our remarkable induction heating solutions to solve our clients' shrink-fitting challenges.
Induction's Benefits for Your shrink-fitting Process:
-
Rapid: Enjoy instant-on heating.
-
Precise & Repeatable: Get the same results every time.
-
Efficient: Apply heat only where it's needed.
-
Safety: Stop using open flame.
We respect your privacy
and will only use the information you provide to administer your account and to deliver the materials you requested.
Four Ways To Contact Ambrell for Support
AMBRELL CORPORATION
1655 Lyell Avenue
Rochester, NY 14606
United States
F: +1 585 889 4030
AMBRELL B.V.
Holtersweg 1
7556 BS Hengelo
The Netherlands
AMBRELL Ltd.
Unit 6, Space Business Centre
Tewkesbury Road
Cheltenham, GLOS, GL51 9FL
United Kingdom
F: +31 546 788 154