In this note...
A dual four turn pancake coil is used to solder 2 brass caps per cycle. Liquid solder is squirted onto the end cap and is heated for 18 seconds at 302°F (150°C) to burn off the flux
Get your Free soldering Application Note
'Soldering Brass end cap on heat exchanger'
See how we've applied our remarkable induction heating solutions to solve our clients' soldering challenges.
We respect your privacy
and will only use the information you provide to administer your account and to deliver the materials you requested.